강추!! ESUN PLA 매트 3D 프린터 필라멘트

-60%
$ 28,100
$ 47,627
4.7/5.0
무료 배송 

ESUN PLA 매트 3D 프린터 필라멘트, 3D 프린터용 3D 인쇄 재료, 1.75mm 치수 +/- 0.03mm, 1kg (2.2 LBS) 스풀

상품 정보

여러분께 소개할 이 제품은 ESUN PLA 매트 3D 프린터 필라멘트으로, 여러분의 생활을 더욱 편리하고 풍요롭게 만들어 줄 것입니다. 아래에서 제품의 특징, 사용 방법, 그리고 왜 이 제품이 여러분에게 이상적인지에 대한 상세한 정보를 제공하겠습니다. 정성껏 준비한 상품 설명을 통해, 여러분이 필요로 하는 최적의 선택을 할 수 있도록 도와드릴 것입니다.


eSUN 3D Printer Filament ePLA-Matte 1.75mm Dimensional Accuracy +/- 0.03mm 1KG (2.2 LBS) Spool 3D Printing Material For 3D Printers

Material:ePLA-Matte

Color:White,Black,Yellow,Grey,Pink,Green

Filament Diameter: 1.75mm

Print Temperature:190-230°C

Print Speed: 40 - 100mm/s

Heat-Bed Temperature: 60°C

Density: 1.26g/m3

Net Weight: 1KG(2.2LBS)

NOTICE: 3D Printing Troubleshooting Guide is at the bottom of the detail page.

3D Printing Troubleshooting Guide

Nozzle clog &Poor extrusion output

Obvious issues(as below)

Suggested solutions:

1. When we met these situations, it is recommended that the printing temperature should raise to 230 ℃, adjust printing speed to 40mm/s, reduced the layer thickness to 0.1mm, then test if it works.

2. If the first step can not solve the problem, need to exclude hardware problems: pull out the front end of the PTFE Pipe Hose to check if it is darken or not , if yes, need replace a new one with nozzle together, because the pipe is already aging.(When replacing, notice that the nozzle need to be tightened with heat)

3. Check the extruder gears, whether the bite is normal, it is recommended that in the case of normal feeding, try to loose the extruder spring.

Non-stick platform, warped edges

Obvious issues(as below)

Suggested solutions:

1. It is recommended to re-level first, the nozzle is too close to the platform will cause the first layer easy to overflow, if too far the first layer can not stick to the platform; if the four corners leveling difference is too large, it may lead to warp from a farther corner.

2. Adjust slicing parameters, the first layer extrusion rate is recommended to be set higher than 100%, the first layer speed set to 10mm/s (refer to the figure below), close the first layer blowing fan, the platform should set to 45-60℃, raft and brim should also adjust to improve the platform's adhesion.

3. If these measures can not solve the problem, it is recommended that the platform coated with PVP solid glue or 3DLac Spray to increase

material adhesion, some lattice base plate may not stick, it can be replaced with pure glass base plate, the adhesion will be better.

4. Winter temperature is too low, PLA-Type materials may also be warped, you can properly open the air conditioner or use eSUN eEnclosure to print or properly reduce the speed of the blowing fan, such as adjusting to 50%.